10298 240402-K3-1

Type: Sample

ObjectId: 69954 ExternalId: 10298

Created: 4/2/2024 1:20:55 PM by Marx Patrick [patrick.marx-l69@rub.de]

Updated: 9/16/2026 4:27:19 PM by Dudarev Victor gmail [vic.dudarev@gmail.com]

Access: Public Sort Code (asc): 0

License: CC BY 4.0

Description: La-Co-V-O hot deposition 500°C on Si/SiO2 with 50 nm Pt and 10 nm Ta adhesion layer, La2O3: RF, 200W, 20W/min ramp, V: pulsed DC, 120W, 350kHz, 1.4µs, Co: DCXS-750, 70W, preanneal 1h

[no file attached]

: Co-La-O-V

Handovers

No handover events found.

Associated Objects

Referenced Objects (Reverse Association)

  • 10293 240327-K3-1
    Sample

    La-Co-V-O hot deposition 500°C, La2O3: RF, 200W, 20W/min ramp, V: pulsed DC, 120W, 350kHz, 1.4µs, Co: DCXS-750, 70W, preanneal 1h

All properties (except table)

Include all template properties
Type Name Value Comment
Int Type 1 Type of the physical sample --//required

The table